Abstract
Ïã¸ÛÁùºÏ²Ê¿ª½± 4802-2:2016 specifies:
a) methods for determining the hydrolytic resistance of the interior surfaces of glass containers when subjected to attack by water at (121 ± 1) °C for (60 ± 1) min. The resistance is measured by determining the amount of sodium and other alkali metal or alkaline earth oxides in the extraction solution using flame atomic emission or absorption spectrometry (flame spectrometry);
b) a classification of glass containers according to the hydrolytic resistance of the interior surfaces determined by the methods specified in Ïã¸ÛÁùºÏ²Ê¿ª½± 4802-2:2016.
The test method specified in Ïã¸ÛÁùºÏ²Ê¿ª½± 4802-2:2016 might not be applicable to containers whose surfaces have been treated with silicon (e.g. containers that are ready for direct filling).
General information
-
Status: WithdrawnPublication date: 2016-06Stage: Withdrawal of International Standard [95.99]
-
Edition: 3Number of pages: 14
-
Technical Committee :Ïã¸ÛÁùºÏ²Ê¿ª½±/TC 76ICS :71.040.20
- RSS updates
Life cycle
-
Previously
WithdrawnÏã¸ÛÁùºÏ²Ê¿ª½± 4802-2:2010
-
Now
-
Revised by
PublishedÏã¸ÛÁùºÏ²Ê¿ª½± 4802-2:2023
Opening hours:
Monday to Friday - 09:00-12:00, 14:00-17:00 (UTC+1)